Strength

max. 215 HB
(≈ 710 N/mm²)

Chemical composition

Thermal conductivity at 20 °C

50 W/(mK)

Character

Unalloyed tool steel with excellent machinability; case hardening steel, suitable for flame and inductive hardening

Application

Machining

Unusual:
Polishing, etching, EDM, nitriding, hard chrome plating

Heat treatment

Soft annealing:
680 to 710 °C, about 2 to 5 hours
Slow, controlled cooling inside the furnace of 10 to 20 °C per hour to about 600 °C
Further cooling in air, max. 190 HB

Hardening:
800 to 830 °C
Quenching in water
Obtainable hardness: 58 HRC
Hardening depth: 3−5 mm
Max. 15 mm through-hardenable

Tempering:
Slow heating to tempering temperature immediately after hardening, to 180 to 300 °C depending on desired hardness
1 hour per 20 mm: at least 2 hours

Choix boutique

Construction d’outils de découpe
Construction d’outils de découpe
Construction de machines et de gabarits
Construction de machines et de gabarits

Aperçu du panier

Aperçu CAD

Votre panier est vide.
Montant net
Vers le panier