1.1730 Tool steel

Our selected range provides the right material for any application.

Products

Characteristics

Designation

Strength

max. 215 HB
(≈ 710 N/mm²)

Chemical composition

Thermal conductivity at 20 °C

50 W/(mK)

Character

Unalloyed tool steel with excellent machinability; case hardening steel, suitable for flame and inductive hardening

Application

Machining

Unusual:
Polishing, etching, EDM, nitriding, hard chrome plating

Heat treatment

Soft annealing:
680 to 710 °C, about 2 to 5 hours
Slow, controlled cooling inside the furnace of 10 to 20 °C per hour to about 600 °C
Further cooling in air, max. 190 HB

Hardening:
800 to 830 °C
Quenching in water
Obtainable hardness: 58 HRC
Hardening depth: 3−5 mm
Max. 15 mm through-hardenable

Tempering:
Slow heating to tempering temperature immediately after hardening, to 180 to 300 °C depending on desired hardness
1 hour per 20 mm: at least 2 hours

Επιλογή καταστήματος

Κατασκευή κοπτικών/διαμορφωτικών καλουπιών
Κατασκευή κοπτικών/διαμορφωτικών καλουπιών
Κατασκευή μηχανημάτων και εξαρτημάτων
Κατασκευή μηχανημάτων και εξαρτημάτων

Προεπισκόπηση καλαθιού

Προεπισκόπηση CAD

Το καλάθι σας είναι άδειο.
Καθαρό ποσό συνολικά
Μετάβαση στο καλάθι

Σημαντική υπόδειξη

Θέλετε να διαμορφώσετε ένα είδος που ανήκει στο . Μετά τις προσαρμογές σας, ελέγξτε μόνοι σας όλες τις πλάκες και τα εξαρτήματα ως προς την τεχνική τους συμβατότητα.