1.7225 Steel for quenching and tempering

Our selected range provides the right material for any application.

Products

Characteristics

Designation

Strength

max. 217 HB
(≈ max. 740 N/mm²)

Chemical composition

Thermal conductivity at 20 °C

42.6 W/(mK)

Character

Alloy steel for quenching and tempering with high resistance and high toughness
Universally usable when quenched and tempered as well as case-hardened

Application

Machining

Suited:
Nitriding, EDM, coating

Unusual:
Welding

Use

Jigs and fixtures, base plates, axes, gear shafts, gear wheels

Heat treatment

Normalising:
840 to 880 °C followed by cooling in air; some components need tempering afterwards

Soft annealing:
680 to 720 °C, about 2 to 5 hours
Slow, controlled cooling inside the furnace of 10 to 20 °C per hour to about 600 °C
Further cooling in air, max. 217 HB

Quenching and tempering:
Max. 1,600 N/mm²

Hardening:
820 to 880 °C
Quenching in oil or water
Oil hardening for thin and complex, water hardening for large and simple components
Obtainable hardness: 53−61 HRC

Tempering:
Slow heating to tempering temperature (in order to avoid the formation of cracks) immediately after hardening
At least 60 minutes cooling in air

Seleziona shop

Costruzione stampi per tranciatura
Costruzione stampi per tranciatura
Costruzione di macchine e attrezzature
Costruzione di macchine e attrezzature

Anteprima del carrello

Anteprima CAD

Il Vostro carrello è vuoto.
Importo totale
Vai al carrello