Products
Characteristics
Designation
Strength
132–185 HB
(≈ 450–630 N/mm²)
Chemical composition
Thermal conductivity at 20 °C
40 W/(mK)
Character
Unalloyed structural steel with good weldability
Application
Machining
Welding
Very good weldability due to low carbon content
Unusual:
Polishing, etching, EDM, nitriding, hard chrome plating
Use
For simple applications in mould, die, and jigs and fixtures construction
Heat treatment
650 to 700 °C, about 2 to 5 hours
Slow, controlled cooling inside the furnace of 10 to 20 °C per hour to about 600 °C
Further cooling in air, max. 180 HB
Technical tip
If no welding is required, we recommend 1.1730 ⇒ better machinability despite higher strength