1.0577 Structural steel

Our selected range provides the right material for almost any application.

Products

Characteristics

Designation

Strength

132–185 HB
(≈ 450–630 N/mm²)

Chemical composition

Thermal conductivity at 20 °C

40 W/(mK)

Character

Unalloyed structural steel with good weldability

Application

Machining

Welding
Very good weldability due to low carbon content

Unusual:
Polishing, etching, EDM, nitriding, hard chrome plating

Use

For simple applications in mould, die, and jigs and fixtures construction

Heat treatment

650 to 700 °C, about 2 to 5 hours
Slow, controlled cooling inside the furnace of 10 to 20 °C per hour to about 600 °C
Further cooling in air, max. 180 HB

Technical tip

If no welding is required, we recommend 1.1730 ⇒ better machinability despite higher strength

Forhåndsvisning af indkøbskurv

CAD-forhåndsvisning

Din indkøbskurv er tom.
Netto i alt
Til indkøbskurv

Vigtig note

Du vil konfigurere et element, der hører til . Efter dine justeringer bedes du kontrollere alle plader og normdele uafhængigt for teknisk kompatibilitet.