1.2312 Tool steel

Our selected range provides the right material for any application.

Products

Characteristics

Designation

Strength

280–325 HB
(≈ 950–1,100 N/mm²)

Chemical composition

Thermal conductivity at 100 °C

35 W/(mK)

Character

Alloyed, quenched and tempered tool steel
Excellent machinability even in quenched and tempered condition due to the sulphur addition
High dimensional stability

Application

Machining

Not recommended:
Etching, EDM

Polishing:
Technical polishing possible
For higher surface requirements we recommend 1.2311 or 1.2738

Nitriding:
Increases the steel’s wear resistance

Use

Plates for mould bases and die sets with increased requirements on strength
High-strength machine parts

Heat treatment

Already pre-hardened; usually no heat treatment required

Nitriding:
Before nitriding, stress-relieving heat treatment is recommended at 580 °C (Meusburger standard).

Hardening:
840 to 860 °C

Cooling:
To 180/220 °C in oil/hot bath
Obtainable hardness: 52 HRC

Tempering:
Slow heating to tempering temperature immediately after hardening
Minimum time in furnace: 1 hour per 25 mm part thickness

Technical tip

For increased surface quality requirements use material 1.2311

Selección de la tienda

Vista previa del carrito

Vista previa CAD

Su carrito de la compra está vacío.
Total neto
Ir al carrito