1.2738 TSHH steel for plastic moulds

Our selected range provides the right material for any application.

Products

Characteristics

Designation

Strength

33–38 HRC
(≈ 1,050–1,200 N/mm²)

Chemical composition

Thermal conductivity at 250 °C

41.3 W/(mK)

Character

Modified, quenched and tempered, good polishability and excellent grainability
High thermal conductivity and wear resistance

Application

Machining

Suited:
Hard chrome plating

Ideally suited:
Polishing, etching, EDM, nitriding

Use

Cavity plates without dimension restrictions, with deep cavities and high core loads

Heat treatment

Already pre-hardened; usually no heat treatment required

Soft annealing:
720 °C 1 hour per 25 mm part thickness
Slow, controlled cooling inside the furnace
Maximum 245 HB

Hardening:
880 °C
Maintain curing temperature for 15 to 30 minutes
Cooling in hot bath/oil/compressed gas
Obtainable hardness: 50 HRC

Tempering:
Slow heating to tempering temperature immediately after hardening
Minimum time in furnace: 1 hour per 25 mm part thickness

Technical tip

  • Consistent hardness over the entire cross section
  • Improved weldability
  • Higher toughness than 1.2738

Choix boutique

Construction d’outils de découpe
Construction d’outils de découpe
Construction de machines et de gabarits
Construction de machines et de gabarits

Aperçu du panier

Aperçu CAD

Votre panier est vide.
Montant net
Vers le panier

Remarque importante

Vous souhaitez configurer un article appartenant à . Après avoir effectué vos ajustements, veuillez vérifier vous-même la compatibilité technique de tous les composants et plaques.