Contact

We are gladly available for you from Monday to Friday from 8:00 to 17:00. Use this link to find the contact persons for your region.

Headquarters Wolfurt
+43 5574 6706-0

Your contacts

Shopping cart {{ (warenkorbCtrl.warenkorb.bestellNummer ? (' [' + warenkorbCtrl.warenkorb.bestellNummer + '] ') : '' )}} | {{warenkorbCtrl.warenkorb.items.length}} Items   Change shopping cart

Remark

Picture Items Pcs Single price Total price Total price incl. discount
{{warenkorbItem.produktgruppe.produktname}}

{{warenkorbItem.bezeichnung | artikelBezFilter:warenkorbItem.attributwertEingaben:[{attrPrefix: 'L_', searchPattern: '/...', replacePrefix: '/', replaceSuffix: ''}] }} {{warenkorbItem.bezeichnung | artikelBezFilter:warenkorbItem.attributwertEingaben}}

{{attributwertEingabe.attributBezeichnung}}

     
{{hannexItem.Benennung}}

{{hannexItem.Bezeichnung}}

     

Please log in to see the precalculated prices and continue with the ordering process.

Lowering tension

In our selected range you can find the right material for virtually any application.

M W10PM powder metallurgical steel

DESIGNATION:

EN: HS 10-2-5-8

INDICATORY ANALYSIS:

C1.6
Cr4.8
Mo2.0
V5.0
W10.5
Co8.0

Strength:

max. 285 HB
(≈ max. 970 N/mm²)

THERMAL CONDUCTIVITY AT 100°C:

26 W/m K


CHARACTER:

High-speed steel produced by powder metallurgy with highest compressivestrength, high adhesive wear resistance and excellent toughness, very high workinghardness possible

APPLICATION:

Blocks for eroding, dies, cutting punches and cutting tools for extremely highrequirements, fine blanking punches, embossing tools, cold solid forming


TREATMENT BY:

Polishing:
best metallurgical properties for mirror finish

Nitriding:
highly suited for nitriding

EDM:
highly suited

Coating:
highly suited


HEAT TREATMENT:

Soft annealing:
870 to 900°C for about 2 to 5 hours
slow controlled cooling inside the furnace 10 to 12°C per hour to about 550°C,
further cooling in air, max. 300 HB

Hardening:
curing temperature: see tempering chart
quenching in oil/compressed gas/air/hot bath
obtainable hardness: 68 HRC

Tempering:
slow heating to tempering temperature (in order to avoid formation of cracks)
immediately after hardening;
keep at tempering temperature for at least 1 hour
four tempering cycles are recommended, with cooling to room temperature in
between


TEMPERING CHART:


TECHNICAL TIP:
  • Retains hardness at high temperatures due to highcobalt content
  • Excellent for PVD and CVD coating without risk ofdimensional changes, as the steel is tempered atmore than 520°C

To the mould making overview To the die making overview

Available in the web shop as:
Data sheet M W10 PM

Open PDF

Material grades brochure

Material grades brochure

Material grades poster

Material grades poster

Log in

Are you already a customer?

If you already have access data for the Meusburger portal, please log in here:

Forgot your password?

The newly generated password is already on the way and should arrive soon in your inbox. We wish you a successful day.

Please enter your email address.
We will send you a new password.

Shop selection

Select your country

Locations

Try our new version of 'My account'

Get familiar with our new ‘My account’ section and benefit from numerous advantages.

Now the new ‘My account’ also gives you a direct insight into the next level of the Meusburger portal. Check out all the information and benefits of the portal here.

Get familiar with our new ‘My account’ section and benefit from numerous advantages.

Now the new ‘My account’ also gives you a direct insight into the next level of the Meusburger portal. Check out all the information and benefits of the portal here.

Keep selection
Beta
New version
Current version